2020
DOI: 10.1016/j.eurpolymj.2020.109918
|View full text |Cite
|
Sign up to set email alerts
|

Polymer side-chain modification in methacrylate and styrene copolymers through thiol-thioester dynamic exchange

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
9
0

Year Published

2021
2021
2023
2023

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 12 publications
(9 citation statements)
references
References 58 publications
0
9
0
Order By: Relevance
“…When analyzing the shape of TG and DTG curves, the decomposition of EGDMA-MMA blends proceeded in several stages. The first stage (T max in the range of 121–137 °C corresponding to 2–3% of mass loss) may be related to the evaporation of residual solvents, moisture and unreacted monomers [ 38 , 39 ]. Subsequent maxima of the rate of mass loss (i.e., T max = 245–258 °C with 7–12% of mass loss and T max = 301–320 °C with 55–64% of mass loss) are probably responsible for the degradation of EGDMA, while the maximum rate of mass loss at T max (temperature range of 396–442 °C and 19–27% of mass loss) is related to the distribution of the fragments derived from MMA.…”
Section: Resultsmentioning
confidence: 99%
See 4 more Smart Citations
“…When analyzing the shape of TG and DTG curves, the decomposition of EGDMA-MMA blends proceeded in several stages. The first stage (T max in the range of 121–137 °C corresponding to 2–3% of mass loss) may be related to the evaporation of residual solvents, moisture and unreacted monomers [ 38 , 39 ]. Subsequent maxima of the rate of mass loss (i.e., T max = 245–258 °C with 7–12% of mass loss and T max = 301–320 °C with 55–64% of mass loss) are probably responsible for the degradation of EGDMA, while the maximum rate of mass loss at T max (temperature range of 396–442 °C and 19–27% of mass loss) is related to the distribution of the fragments derived from MMA.…”
Section: Resultsmentioning
confidence: 99%
“…The heat capacity of these transformations for the BPA.GDA blend series decreases with the increasing amount of PC in the material, while for the EGDMA blends the trend is reversed. As shown in the literature, the T g of pure PMMA ranges from 104 to 122 °C and depends on the molar mass of the obtained polymer [ 38 , 42 , 43 ], while the T m of the PMMA is approximately 72 °C [ 44 ]. The broad exothermic peaks (in fact it is a change in slope of curve that comes from an endothermic peak with T recryst at 101 and 107 °C) for BPA.GDA + MMA + 1% PC and BPA.GDA + MMA + 5% PC blends are responsible for the recrystallization of PMMA crystallites or with polymorphic changes in the crystal structure.…”
Section: Resultsmentioning
confidence: 99%