Nanostructure, porosity and tensile strength of PVA/Hydroxyapatite composite nanofiber for bone tissue engineering

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

2
3
0
1

Year Published

2021
2021
2023
2023

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 17 publications
(7 citation statements)
references
References 22 publications
2
3
0
1
Order By: Relevance
“…The successful incorporation of HA was seen in the form of aggregation mass inside the fibre in the case of CNF-HA, and the average diameter was 150.5 ± 24.337 nm. The addition of HA also makes the surface of the fibre rougher, and this result is consistent with those of previous work ( Hartatiek et al, 2021 ). It should be remembered that the embedded HA produces a rough nanofiber surface, which is expected to increase surface wettability and encourage the attachment of bone cells and the formation of new bone differentiation ( Bodhak et al, 2009 ; Hartatiek et al, 2021 ).…”
Section: Resultssupporting
confidence: 93%
See 2 more Smart Citations
“…The successful incorporation of HA was seen in the form of aggregation mass inside the fibre in the case of CNF-HA, and the average diameter was 150.5 ± 24.337 nm. The addition of HA also makes the surface of the fibre rougher, and this result is consistent with those of previous work ( Hartatiek et al, 2021 ). It should be remembered that the embedded HA produces a rough nanofiber surface, which is expected to increase surface wettability and encourage the attachment of bone cells and the formation of new bone differentiation ( Bodhak et al, 2009 ; Hartatiek et al, 2021 ).…”
Section: Resultssupporting
confidence: 93%
“…The addition of HA also makes the surface of the fibre rougher, and this result is consistent with those of previous work ( Hartatiek et al, 2021 ). It should be remembered that the embedded HA produces a rough nanofiber surface, which is expected to increase surface wettability and encourage the attachment of bone cells and the formation of new bone differentiation ( Bodhak et al, 2009 ; Hartatiek et al, 2021 ). Additionally, for CNF-SBG and CNF-BBG, respectively, the fiber diameter increased to (167.5 ± 6.9) nm and (123.5 ± 7.99) nm after silicate and borosilicate bioactive glass doping.…”
Section: Resultssupporting
confidence: 93%
See 1 more Smart Citation
“…The hydroxyapatite (Ca 10 (PO 4 ) 6 (OH) 2 ) was synthesized from limestone [27] The synthesis of PVA/Chitosan/PEG/HAp begins with the preparation of a PVA/Chitosan/PEG solution. First, 1% of chitosan was mixed with 2% of acetic acid and stirred using a magnetic stirrer at a speed of 700 rpm for 2 h at room temperature.…”
Section: Methodsmentioning
confidence: 99%
“…Pemilihan rasio perbandingan PVA:HAp sebesar 5:5, 6:4, 7:3, 8:2, dan 9:1 didasarkan pada penelitian oleh Hartatiek et.al, pada tahun 2021 mengenai komposit PVA/Hidroksiapatit menggunakan variabel serupa dengan hasil terbaik didapatkan pada variabel 7:3 [22]. Selain itu kekuatan mekanik, morfologi dari komposit juga dapat dimanipulasikan menggunakan variabel tersebut, dikarenakan ikatan silang kimia dari polimer PVA yang juga memberikan pengaruh kepada kekuatan mekanik komposit [23].…”
Section: Sifat Mekanik Kompositunclassified