2016
DOI: 10.2109/jcersj2.15190
|View full text |Cite
|
Sign up to set email alerts
|

Hot-pressed laminated composites consisting of ZrB<sub>2</sub>&ndash;SiC ceramic and Cf/ZrB<sub>2</sub>&ndash;SiC composites

Abstract: In this study, laminated composites consisting of ZrB 2 SiC (ZS) ceramic and carbon fiber (Cf ) reinforced-ZrB 2 SiC matrix composites (Cf/ZrB 2 SiC, hereafter denoted by CfZS) were fabricated by hot-pressing. The effects of the layer thickness ratio of ZS to CfZS (ZS/CfZS) and the fiber concentration on the flexural strength were investigated. The flexural strength of the laminated composites was improved compared to that of the single-composites and the improvement was enhanced with increase of the ZS/CfZS r… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
2
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(2 citation statements)
references
References 24 publications
(10 reference statements)
0
2
0
Order By: Relevance
“…Several studies have previously investigated the fracture behavior of ZrB 2 based laminate composites 36–41 . Zhou et al described ZrB 2 ‐SiC based laminates prepared by hot‐pressing with flexure strength of 960 MPa and fracture toughness of 8.8 MPa·m ½ , though exhibiting relatively low amounts of crack deflection 36 .…”
Section: Introductionmentioning
confidence: 99%
“…Several studies have previously investigated the fracture behavior of ZrB 2 based laminate composites 36–41 . Zhou et al described ZrB 2 ‐SiC based laminates prepared by hot‐pressing with flexure strength of 960 MPa and fracture toughness of 8.8 MPa·m ½ , though exhibiting relatively low amounts of crack deflection 36 .…”
Section: Introductionmentioning
confidence: 99%
“…due to its inherent brittleness and poor thermal shock resistance. Thus, a variety of reinforcements, such as particles [3], graphite flakes [4], whiskers [5], and fibers [6][7][8][9], have been adopted to toughen ZrB 2 ceramics via different toughening mechanisms. Carbon fiber has been widely researched as a toughening material for the ZrB 2 -based UHTCs due to its large aspect ratio and good high-temperature stability.…”
mentioning
confidence: 99%