“…The initial decomposition temperatures increase with f LG , reaching 430, 438, 439, 440, 442, 443, and 443 °C for the pure PVDF and the LG/PVDF nanocomposites with f LG = 0.02, 0.04, 0.06, 0.08, 0.09, and 0.10, respectively. The thermal degradation after reaching 470 °C was primarily attributed to the cleavage of oxygen-containing functional groups and grafted molecular chains . Thus, the addition of LG filler can improve the thermal stability of PVDF polymer by increasing the decomposition temperature of LG/PVDF nanocomposites, as shown in the inset of Figure c.…”