Fabrication of 3D-interconnected microporous carbon decorated with microspheres for highly efficient hydrogen evolution reactions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
0
0

Year Published

2024
2024
2024
2024

Publication Types

Select...
2

Relationship

1
1

Authors

Journals

citations
Cited by 2 publications
(1 citation statement)
references
References 45 publications
0
0
0
Order By: Relevance
“…During pyrolysis, the furnace temperature was increased stepwise to 1000 °C and maintained for 4 h at this temperature. The stepwise gradual increase of furnace temperature was optimized and reported in our previous experiment [35]. The LIG-CF electrode was obtained after natural cooling to room temperature, e.g., 25 °C.…”
Section: Methodsmentioning
confidence: 99%
“…During pyrolysis, the furnace temperature was increased stepwise to 1000 °C and maintained for 4 h at this temperature. The stepwise gradual increase of furnace temperature was optimized and reported in our previous experiment [35]. The LIG-CF electrode was obtained after natural cooling to room temperature, e.g., 25 °C.…”
Section: Methodsmentioning
confidence: 99%