Effects of Si addition on the glass-forming ability, glass transition and crystallization behaviors of Ti40Zr10Cu36Pd14 bulk glassy alloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
20
0

Year Published

2009
2009
2020
2020

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 21 publications
(21 citation statements)
references
References 25 publications
1
20
0
Order By: Relevance
“…The value of activation energy E p was calculated as 334.3 kJ/mol which was higher than that of the TiZrCuPd glassy alloy without Sn addition (287.6 kJ/mol). 14) This indicates the improvement of thermal stability due to the Sn addition. The TiCu phase is considered as preferable crystallized phase for the TiCu-rich bulk glassy alloys.…”
Section: Resultsmentioning
confidence: 89%
See 2 more Smart Citations
“…The value of activation energy E p was calculated as 334.3 kJ/mol which was higher than that of the TiZrCuPd glassy alloy without Sn addition (287.6 kJ/mol). 14) This indicates the improvement of thermal stability due to the Sn addition. The TiCu phase is considered as preferable crystallized phase for the TiCu-rich bulk glassy alloys.…”
Section: Resultsmentioning
confidence: 89%
“…14) Ti-based bulk glassy alloys are expected to be applied as biomaterials because of their excellent corrosion resistance, good biocompatibility, low Young's modulus and high recovery of strain (>2%). Some of works have been made for Ti-based bulk glassy alloys, such as TiNiCu, 5) TiNiCuCo, 6) TiCuNiSn, 7) TiZr CuNi 8) and others TiBe-based 9) systems.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…8288) Niand Be-free Ti-based (Ti 45 Zr 10 Cu 31 Pd 10 Sn 4 ) atomized glassy powder was consolidated by the SPS process at various sintering temperatures. The samples sintered by the SPS process at a sintering temperature of 643 K with a loading pressure of 600 MPa exhibited high strength, high densification and a full glassy structure, and the potentiodynamic polarization curve showed a flat passive region after active dissolution at open-circuit potential, having a higher pitting potential.…”