2019
DOI: 10.1016/j.jallcom.2019.04.137
|View full text |Cite
|
Sign up to set email alerts
|

Effect of varying TiB2 reinforcement and its ageing behaviour on tensile and hardness properties of in-situ Al-4.5%Cu-xTiB2 composite

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

2
15
0

Year Published

2019
2019
2022
2022

Publication Types

Select...
5
4

Relationship

0
9

Authors

Journals

citations
Cited by 81 publications
(18 citation statements)
references
References 31 publications
2
15
0
Order By: Relevance
“…7 Aluminum composites possessing in situ TiC and TiB 2 reinforcements are gaining enough attention lately because of its high hardness, elastic modulus and resistance to wear. [8][9][10] A reduction in inter dendritic arm spacing has also been found in the in situ reinforcement. During the solidification of base alloy, these reinforcing phase acts as a nucleation sites for the growth of dendritic arms, hence improves the wettability of the reinforcing phase.…”
Section: Introductionmentioning
confidence: 73%
“…7 Aluminum composites possessing in situ TiC and TiB 2 reinforcements are gaining enough attention lately because of its high hardness, elastic modulus and resistance to wear. [8][9][10] A reduction in inter dendritic arm spacing has also been found in the in situ reinforcement. During the solidification of base alloy, these reinforcing phase acts as a nucleation sites for the growth of dendritic arms, hence improves the wettability of the reinforcing phase.…”
Section: Introductionmentioning
confidence: 73%
“…The utility measure for the rate of material removal is calculated using equation 9, whereas overcutting and delamination are computed using equation (10). Furthermore, the regret measure is estimated using equation (11). The VIKOR index is calculated by inserting the utility and regret measure values into equation 12(see Table 4).…”
Section: Resultsmentioning
confidence: 99%
“…10 Not long ago, the synthesis of aluminium composites reinforced with TiB 2 using K 2 TiF 6 -KBF 4 -aluminium melt reactions and the evaluation of mechanical properties under various treating conditions received the attention of researchers worldwide. [11][12][13] AA6061-TiB 2 composites have several beneficial effects. For example, the TiB 2 particulates act as a diverse nucleation region and facilitate the fine grain size of aluminium.…”
Section: Introductionmentioning
confidence: 99%
“…In the case of ceramic-reinforced metal matrix composites, when tension is applied in the vertical direction to composites in which soft Al, having low strength, is present, the material stretches, and fractures proceed as defects are formed at interface between reinforcements and the matrix. If this interface is not sound, the reinforcements-matrix interface plays a major role in the formation of defects such as voids [31]. Therefore, composites having poor interfaces may exhibit poor mechanical properties due to interfacial delamination.…”
Section: Mechanical Properties Of Tib 2 -Al1050 Compositesmentioning