Abstract: Synthetic V bearing steelmaking slags with different contents of TiO 2 were solidified from melting temperature of 1530uC. The effect of TiO 2 on the crystallisation temperature and crystal growth of V concentrating phase is clarified by SEM and EDX and analysis of crystal size distribution. Results show that 2?2-4?2 wt-%TiO 2 can lower the crystallisation temperature from 1350 to 1275uC and crystal growth is enhanced but not linearly with the addition of TiO 2 .

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

4
28
0

Year Published

2009
2009
2018
2018

Publication Types

Select...
8
1
1

Relationship

0
10

Authors

Journals

citations
Cited by 31 publications
(32 citation statements)
references
References 9 publications
(10 reference statements)
4
28
0
Order By: Relevance
“…Thus, the dynamics condition for vanadium-extraction becomes worse, and the yield ratio of vanadium is decreased. [11][12][13][14] Though the viscosity of Cr 2 O 3 -bearing slag would decease with increasing of the temperature, the oxidation of vanadium would be suppressed according to the selective oxidation theory, and thus the practical blowing smelting temperature is usually controlled below 1 653 K. [15][16][17] Therefore, study on the influence of Cr 2 O 3 on the properties of FeO-SiO 2 -V 2 O 3 (-TiO 2 ) system slag is very important to improve the blowing smelting technology for the vanadium-extraction from the chromiumbearing hot metal.…”
Section: Viscosity Property and Structure Analysis Of Feo-sio 2 -V 2 mentioning
confidence: 99%
“…Thus, the dynamics condition for vanadium-extraction becomes worse, and the yield ratio of vanadium is decreased. [11][12][13][14] Though the viscosity of Cr 2 O 3 -bearing slag would decease with increasing of the temperature, the oxidation of vanadium would be suppressed according to the selective oxidation theory, and thus the practical blowing smelting temperature is usually controlled below 1 653 K. [15][16][17] Therefore, study on the influence of Cr 2 O 3 on the properties of FeO-SiO 2 -V 2 O 3 (-TiO 2 ) system slag is very important to improve the blowing smelting technology for the vanadium-extraction from the chromiumbearing hot metal.…”
Section: Viscosity Property and Structure Analysis Of Feo-sio 2 -V 2 mentioning
confidence: 99%
“…1,2 Vanadium exists mainly in the form of titaniferrous magnetite. The major vanadium products include ferrovanadium (FeV), V 2 O 5 , V 2 O 3 , VN and Al-V-Ti alloy.…”
Section: Introductionmentioning
confidence: 99%
“…Therefore, in order to enhance the phosphorus content in the enriched phase, the steelmaking slags were usually modified by different additives, such as Al 2 O 3 , SiO 2 and TiO 2 , to explore the microstructure and the enhancement of the solubility of phosphorus enriched phase. 4,5,11) Although there exists extensive literatures studying the effect of fluorine on the dephosphorus process, 12,13) the effects on the viscosity and crystallization are limited; and the kinetics of the precipitation during the continuous cooling has not been documented.…”
Section: Viscous Flow and Crystallization Behaviors Of P-bearing Steementioning
confidence: 99%