2012
DOI: 10.1016/j.polymertesting.2012.01.003
|View full text |Cite
|
Sign up to set email alerts
|

AFM nanoindentation to determine Young’s modulus for different EPDM elastomers

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

3
44
0
2

Year Published

2015
2015
2022
2022

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 64 publications
(49 citation statements)
references
References 21 publications
3
44
0
2
Order By: Relevance
“…The load-penetration depth curve can be used together with a contact mechanics model to calculate the stiffness of the sample. This technique has been successfully applied to both polymers and rubbers [26][27][28]. The viscoelastic properties of the samples can be obtained by performing measurements at various temperatures and/or indentation ratios [29,30].…”
Section: Nanoscale Mechanical Characterizationmentioning
confidence: 99%
“…The load-penetration depth curve can be used together with a contact mechanics model to calculate the stiffness of the sample. This technique has been successfully applied to both polymers and rubbers [26][27][28]. The viscoelastic properties of the samples can be obtained by performing measurements at various temperatures and/or indentation ratios [29,30].…”
Section: Nanoscale Mechanical Characterizationmentioning
confidence: 99%
“…In this model, it is assumed that the indenter tip is not deformable and thus it does not change during the measurement and that the Young's modulus for the indenter tip is much larger than the Young's modulus for the sample. The Hertz model for a sharp cone of tip angle 2c yields to the following equa-tion for the load force, F as a function of the indentation depth, ı (Bulychev, Alekhin, Shorshorov, Ternovskii, & Shnyrev, 1975;Ferencz, Sanchez, Blumich, & Herrmann, 2012;Lin, Dimitriadis, & Horkay, 2007),…”
Section: Characterizationmentioning
confidence: 99%
“…Another way to probe changes in the mechano-elastic properties that are modified by the addition of RTILs is offered by AFM. Both the Young's moduli and the rupture forces can be determined for single supported phospholipid bilayers and vesicles (Monocles et al 2010; Garcia-Manyes and Sanz 2010; Roa et al 2011;Ferenc et al 2012;Stetter et al 2016;Ding et al 2017). To the best of our knowledge, there are no AFM studies of this kind.…”
Section: Introductionmentioning