volume 34, issue 1, P33-41 1994
DOI: 10.1002/pen.760340109
View full text
|
|
Share

Abstract: Abstract Nylon 6 has been toughened by rubber particles that were dispersed within the matrix via additives that physically interact with the elastomer phase but chemically react with the polyamide phase. To disperse a core‐shell impact modifier having a poly(methyl methacrylate) or PMMA shell, most of the work presented is based on the use of a styrene/acrylic acid copolymer containing 8 wt% acrylic acid, SAA8. SAA8 is miscible with PMMA and should located in the PMMA grafted chains of the impact modifier wh…