Abstract: Crystallinity is an important property of lignocellulosic biomass due to its significant effect on acid/enzymatic hydrolysis. Normally, physicochemical analysis, such as powder X-ray diffraction and nuclear magnetic resonance, is used to reveal the crystallinity content. However, these analytical methods are expensive and laborious. In this context, methods that rapidly predict the crystallinity are important, even if used only for screening calibration. Thus, we intend to show the potential of near-infrared s… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

2
22
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 28 publications
(24 citation statements)
references
References 1 publication
2
22
0
Order By: Relevance
“…The olive mill residue showed the highest CrI (55.8%), while in citrus waste biomass it was less than 20% (Figure 2). These values are consistent with those previously reported for agrifood residue [13,45,46].…”
Section: Crystallinitysupporting
confidence: 93%
“…The olive mill residue showed the highest CrI (55.8%), while in citrus waste biomass it was less than 20% (Figure 2). These values are consistent with those previously reported for agrifood residue [13,45,46].…”
Section: Crystallinitysupporting
confidence: 93%
“…The crystalline index revealed a 64% of crystallinity for holocellulose, which is similar to those found for hollocellulose extracted from flax stem, rose stems and banana peels [42,47,48]. However, crystalline index of cellulose II was 83%, which was better than that obtaneid for cellulose II extracted from sago seed shells, sugarcabe bagasse, alfa fibers and red algae waste [44,49].…”
Section: Resultssupporting
confidence: 59%
“…XRD analysis on WCCB, extracted wax, and char were performed on a Siemens D5000 diffractometer using Cu‐Ka radiation (0.1542 nm) from 2 θ = 2 to 80° at 0.01° steps. The crystallinity index (CI) for cellulose (CI c ) and wax (CI w ) were determined using the adjusted deconvolution method 26,27 CI=()AitaliccryAcry+Aitalicam×100 where A cry is the adjusted crystalline peak area, and A am is the adjusted broad peak area of the amorphous component.…”
Section: Methodsmentioning
confidence: 99%