Abstract: Friction stir welding was used to produce butt joints on 6 mm thick plates of UNS S32101 lean duplex stainless steel, S32205 duplex stainless steel, and S32750 and S32760 superduplex stainless steels. Fully consolidated joints were achieved, with full penetration, using heat input of 1.37-1.50 kJ/mm. Specimens submitted to tensile testing performed perpendicular to the welding direction showed failure on the base metal, reflecting better mechanical performance of the welded joints. Furthermore, tensile testing… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
13
0
7

Year Published

2016
2016
2018
2018

Publication Types

Select...
7
1

Relationship

1
7

Authors

Journals

citations
Cited by 34 publications
(20 citation statements)
references
References 37 publications
(48 reference statements)
0
13
0
7
Order By: Relevance
“…Both of them can produce a recrystallization process, which is followed by grain growth in the ferrite phase. According to earlier studies, DRX, including continuous DRX (CDRX), or discontinuous DRX (DDRX) may exist in the SZ during the FSW of DSSs [24][25][26]29,30]. High stacking fault energy (SFE) of the ferrite phase facilitates CDRX.…”
Section: Microstructural Evolutionmentioning
confidence: 99%
“…Both of them can produce a recrystallization process, which is followed by grain growth in the ferrite phase. According to earlier studies, DRX, including continuous DRX (CDRX), or discontinuous DRX (DDRX) may exist in the SZ during the FSW of DSSs [24][25][26]29,30]. High stacking fault energy (SFE) of the ferrite phase facilitates CDRX.…”
Section: Microstructural Evolutionmentioning
confidence: 99%
“…O torque resultante na junta é governado pelas características de fluxo dos materiais a serem soldados, e pela velocidade do fuso. Dessa forma, a menor força axial, combinada com maior velocidade de rotação e menor velocidade de avanço resulta em menor torque na junta soldada, pois proporciona maior entrada de calor, o que aumenta a fluidez do material [22].…”
Section: Reações Relevantes Ao Processo Friction Stir Weldingunclassified
“…Santos et al [22] soldaram aços inoxidáveis duplex e super duplex de 6 mm de espessura, usando um equipamento Technologies Inc. (TTI), dedicado à soldagem pelo processo FSW. Para as soldagens foi utilizada uma ferramenta de PCBN-40% W-Re com ombro de 25 mm de diâmetro e pino com comprimento de 6 mm e 8 mm de diâmetro.…”
Section: Reações Relevantes Ao Processo Friction Stir Weldingunclassified
“…Os ensaios não foram realizados para o aço UNS S32205 devido à indisponibilidade de amostras de tamanho adequado. A Tabela 3 apresenta os dados obtidos pelos ensaios de tração em amostras do metal de base e em amostras longitudinais nas juntas soldadas [22]. Tabela 3.…”
Section: Ensaios Mecânicosunclassified
“…Tabela 3. Ensaios de tração longitudinais em juntas soldadas [22]. Da análise das superfícies de fratura após os testes de tração, a Figura 6 apresenta as fractografias das juntas soldadas para os aços UNS (a) S32101, (b) S32750 e (c) S32760.…”
Section: Ensaios Mecânicosunclassified