This study determines how levels of various trace metals in wool and the colour of the fibre change as a result of sunlight exposure and treatment with chelating compounds during wool growth. Twenty-four yearling Merino sheep were clipped on the shoulders and rumps and fitted with sheep coats modified with transparent patches. Patches over the shoulder wool (one per sheep) were either polyethylene (PE) that transmits ultraviolet light or polyvinyl chloride (PVC) that excludes ultraviolet light. The rump wool on each sheep was treated either with a copper chelator treatment (kojic acid or methyl gentisate in aqueous alcohol) or aqueous alcohol only. For 12 of the sheep the rumps were exposed to sunlight through PE patches while rump wool on the other sheep was covered by the sheep coat. Wool was harvested after 11 weeks’ growth with yellowness (Y-Z) and individual mineral contents measured using the same clean wool sample. Sunlight exposure through PE patches caused a mean increase in Y-Z to 9.1 (shoulder) or 9.5–10.1 (rump) from a base level of 7.1–7.2 (shoulder) or 7.0–7.6 (rump) in wool protected by the sheep coat. In contrast, there was no significant change in Y-Z for the PVC patch (shoulder). Therefore, it appears that ultraviolet light damage caused the increased Y-Z. Most of the trace metals analysed increased in the shoulder wool exposed to sunlight but the paired differences for PVC were lower than PE. It appears that changes in fibre caused by sunlight exposure (especially ultraviolet light) facilitate adsorption of minerals from the environment, including the animal’s own suint. Application of the chelating compounds to the rump wool caused pronounced yellowing of the wool with Y-Z increase being most pronounced for kojic acid. Copper levels in the wool were reduced by kojic acid and methyl gentisate while calcium levels were increased by kojic acid and reduced by methyl gentisate. It is not clear from these findings whether minerals and copper in particular contribute to yellowing of wool. However, the different effects of sunlight and chelation on mineral contents in wool shown may well relate to alternative mechanisms of discoloration (i.e. photoyellowing versus bacterial).
A convenient method for measuring the clean colour (Y and Y-Z) and photostability Δ(Y-Z) of small samples of fleece wool (0.5 g) is described. Scoured wool samples are compressed to a constant density in disposable polymethyl methacrylate spectrophotometer cells and the wool colour is measured using a standard textile laboratory reflectance spectrophotometer. Packing scoured wool into cells ensures that the irradiated fibre surface is robust and individual fibres are unable to move relative to one another during irradiation and measurement. A UVB (280–320 nm) source was used to ensure all samples regardless of initial yellowness were yellowed following exposure and photobleaching was avoided. An apparatus capable of irradiating up to 48 scoured wool samples in one batch is described. The precision of photostability measurements was assessed and the relative error in Δ(Y-Z) was 5.7%. An initial study on 75 fleece wool samples with a high range of initial yellowness showed a moderate linear correlation (R2 = 0.68) between initial yellowness and Δ(Y-Z).
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
hi@scite.ai
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.